Produce No | Glass | Weight(g/m²) | ≥N/25MM Breaking Strength | Weave | % Moisture
Content |
% L.O.I
Content |
|
Warp | Weft | ||||||
CWR140 | C | 140+/-7 | 345 | 315 | Plain | ≤0.2 | 0.4-0.8 |
EW100 | E | 100+/-5 | 460 | 400 | Plain | ≤0.1 | 0.4-0.8 |
EW130 | E | 130+/-7 | 700 | 460 | Plain | ≤0.1 | 0.4-0.8 |
EW160 | E | 160+/-8 | 700 | 680 | Plain | ≤0.1 | 0.4-0.8 |
EWR200A | E | 200+/-10 | 800 | 710 | Plain | ≤0.1 | 0.4-0.8 |
EWR250TK | E | 250+/13 | 1600 | 1500 | Twill | ≤0.1 | 0.4-0.8 |
EWR300TK | E | 300+/-15 | 2000 | 1700 | Twill | ≤0.1 | 0.4-0.8 |
EWR40OTK | E | 400+/-20 | 2500 | 1450 | Twill | ≤0.1 | 0.4-0.8 |